Show full item recordAbstract
Spray Pyrolysis Technique (SPT) was used to deposit thin films (TFs) of cadmium stannate, doped
with iron (Fe) for the first time. The precursor solutions that were used wereprepared at a concentration of
0.1M, doped with Feand then sprayed onto the pre-heated glass slides immediately at deposition temperatures
of 350 ± 7°C, 400 ± 7°C and 450 ± 7°C. The optical properties of the deposited Fe-doped TFs were studied in
the wavelength range of 300-1100nm. The X-Ray diffraction (XRD) studies showed that the TFs were
orthorhombic with growth orientation along the (2 0 0) direction. Film thickness of 85 ± 10 nm was obtained. It
was found out that anincrease in the deposition temperature increased transmittance and band gap, but
decreased absorption coefficient, extinction coefficient and refractive index, which was attributed to the
improvement in crystallinity of the deposited TFs. Doping reduced transmittance and band gap, but increased
refractive index, absorption coefficient and extinction coefficient, which was attributed to the increase in free
carriers
Citation
Ongwen, Nicholas O., Erick Ogam, and Henry O. Otunga. "Ab initio study of elastic properties of orthorhombic cadmium stannate as a substrate for the manufacture of MEMS devices." Materials Today Communications 26 (2021): 101822.Publisher
University of Nairobi
Subject
cadmium stannate, deposition temperature, iron-doped, optical properties of cadmium stannate.Rights
Attribution-NonCommercial-NoDerivs 3.0 United StatesUsage Rights
http://creativecommons.org/licenses/by-nc-nd/3.0/us/Collections
The following license files are associated with this item: